Use of Rejected/Burn Core Sand in Foundry for Cold Box Core Making through Innovative Approach

0 0 /5
In Swaraj Foundry, castings are made for Swaraj tractor. Silica sand cores are used for making internal parts of casting. During Core making process rejection is 5% weighing 5000 kg/day. After placing core into mold, liquid metal is poured at 1400°C. Organic binders burn away resulting disintegration of cores.